Nickel-based superalloy powder for 3D printing

Product NO.In718(GH4169)、In 625(GH3625)

Category3D Printing Materials

ProfileNickel-based superalloy powder for 3D printing

Product description

Nickel-based superalloy powder for 3D printing


category

Alloy grades and characteristics

Alloy number:

In718(GH4169)、In 625(GH3625)、Hastelloy X (GH3536)、Waspaloy(GH738)、In713C(K418)、K465、K640、Rene′125(DZ125)、DD6、FGH95、FGH96、FGH97


Particle size:

0-20μm, 15-45μm, 15-53μm, 53-105μm, 53-150μm, 105-250μm

Morphology:

Spherical or nearly spherical

Appearance:

Grey 

Package:

Aluminum bag,Vacuum packing

Application:

3D printing metal powder

Other applications:

powder metallurgy(PM), injection molding(MIM), spray painting(SP) etc.



Alloy number

Material forming process and state

Mechanical property

σb(MPa)

σ0.2(MPa)

δ(%)

IN718


Precinct laser melting/sintering heat treatment

1350-1500


1140-1280

9-20

Laser melt forming heat treatment state

1340-1360

1130-1170

16-28

Forging annealing standard reference

≥1280

≥1040

≥12

IN625


Precinct laser melting/sintering heat treatment

830-1140

550-820

30-40

Forging annealing standard reference

≥830

≥410

≥30




Luoyang Tongrun Info Technology Co., Ltd. is committed to technology development, applications of nanotechnology and new material industries, with professional experience in the nano-technology research and development and the application of materials.  As a leading nano-technology development and product applications manufacturer, the Luoyang Tongrun dominates the markets. Tongrun technology provides solutions across the various processes and steps of laboratories and industries. Our professional working team provides the perfect solutions to help increase efficiency in various industries, create value, easy to deal with various challenges.

Currently our company has successfully developed serious of powder materials (including oxides, carbides, nitrides, single metal, etc.), high-purity target, functional ceramics and structural devices. OEM service is available. And our innovative, high-performance materials are widely used in all aspects of daily life, including but not limited to the automotive, electrical, electronics, information technology, petrochemical, oil, ceramics, paint, metallurgy, solar energy and catalysis.


Newsletter

Your Name:

Your Company:

Your E-mail:

Verification Code: