Aluminum-based superalloy powder for 3D printing


categoryAlloy grades and characteristics
Alloy number:221920246061AlSi7MgZL101AlSi12ZL102AlSi10MgZL104Al-Si5Cu1MgZL105
Particle size:0-20m, 15-45m, 15-53m, 53-105m, 53-150m, 105-250m
Morphology:Spherical or nearly spherical
Appearance:Grey
Package:Aluminum bag,Vacuum packing
Application:3D printing metal powder
Other applications:powder metallurgy(PM), injection molding(MIM), spray painting(SP) etc.



Alloy numberMaterial forming process and stateMechanical property


bMPa0.2MPaģ%
AlSi10Mg Aluminum alloy powderPrecinct laser melting/sintering heat treatment280-350170-2208-18

Forging annealing standard reference3001703.5



Luoyang Tongrun Info Technology Co., Ltd. is committed to technology development, applications of nanotechnology and new material industries, with professional experience in the nano-technology research and development and the application of materials.  As a leading nano-technology development and product applications manufacturer, the Luoyang Tongrun dominates the markets. Tongrun technology provides solutions across the various processes and steps of laboratories and industries. Our professional working team provides the perfect solutions to help increase efficiency in various industries, create value, easy to deal with various challenges.

Currently our company has successfully developed serious of powder materials (including oxides, carbides, nitrides, single metal, etc.), high-purity target, functional ceramics and structural devices. OEM service is available. And our innovative, high-performance materials are widely used in all aspects of daily life, including but not limited to the automotive, electrical, electronics, information technology, petrochemical, oil, ceramics, paint, metallurgy, solar energy and catalysis.